Tumbling brass
Moderator: dromia
Forum rules
All handloading data posted on Full-Bore UK from 23/2/2021 must reference the published pressure tested data it was sourced from, posts without such verification will be removed.
Any existing data without such a reference should be treated as suspect and not used.
Use reloading information posted here at your own risk. This forum (http://www.full-bore.co.uk) is not responsible for any property damage or personal injury as a consequence of using reloading data posted here, the information is individual members findings and observations only. Always verify the load data and be absolutely sure your firearm can handle the load, especially older ones. If in doubt start low and work your way up.
All handloading data posted on Full-Bore UK from 23/2/2021 must reference the published pressure tested data it was sourced from, posts without such verification will be removed.
Any existing data without such a reference should be treated as suspect and not used.
Use reloading information posted here at your own risk. This forum (http://www.full-bore.co.uk) is not responsible for any property damage or personal injury as a consequence of using reloading data posted here, the information is individual members findings and observations only. Always verify the load data and be absolutely sure your firearm can handle the load, especially older ones. If in doubt start low and work your way up.
Re: Tumbling brass
The media arrived to day I now have bucket loads of the stuff. 

- phaedra1106
- Posts: 3429
- Joined: Wed Feb 08, 2012 9:37 pm
- Location: Just outside Sacriston (the nice bit!)
- Contact:
Re: Tumbling brass
Everyone round to your place for a mass tumbling session this weekend then
:)
Or ....... pile it all together and rent it out as a "Rough Sand Pit and Child Cleaning Area" :)

Or ....... pile it all together and rent it out as a "Rough Sand Pit and Child Cleaning Area" :)
There's room for all Gods creatures, next to the mash and gravy :)
Re: Tumbling brass
Well that was Wednesday night. So if you've forgotten about them, they should be nice and shiny...Alpha1 wrote: Just need to pop the lid on and plug it in and she is off. She is currently burbling away I will check on her later I thought two hours for starters. So watch this space.



Re: Tumbling brass
Some of it is really fine its like sand. I have refilled it and its burbling away again.
Re: Tumbling brass
Well it was a pretty easy experiment in the end for me anyway. As I said in the beginning cleaning brass is not high on my priorities re loading and shooting does it for me. My cases have to be pretty manky before I think about cleaning them.
Any way I settled on two grades of media. This is the one I started off with I will add the grades later. (media 1)It cleaned the brass to an acceptable level they are clean but not super shiny I left them in for 4 hours I did not add anything to the media no polishes etc.Any defects in the cases would be easily picked up. It blocked the flash holes. (The finnish is acceptable to me.
(media 2) I then used this grade of media which is like sand it also cleaned the cases to an acceptable level they are clean but not super shiny. I left them in for four hours I did not add anything to the media to polish etc. Any defects in the cases would be easily picked up. It did not block the flash holes. (The finnish is acceptable to me.)
In future I would probably tumble for four hours with (media 1) and maybe add a polish or jewelers rouge. Probably jewelers rouge.
I would then tumble for two hours in (media2) with jewelers rouge added.
The results are acceptable to me but I know some other people feel the need to be able to use there brass as shaving mirrors so obviously this will not suit them.
Any way I settled on two grades of media. This is the one I started off with I will add the grades later. (media 1)It cleaned the brass to an acceptable level they are clean but not super shiny I left them in for 4 hours I did not add anything to the media no polishes etc.Any defects in the cases would be easily picked up. It blocked the flash holes. (The finnish is acceptable to me.
(media 2) I then used this grade of media which is like sand it also cleaned the cases to an acceptable level they are clean but not super shiny. I left them in for four hours I did not add anything to the media to polish etc. Any defects in the cases would be easily picked up. It did not block the flash holes. (The finnish is acceptable to me.)
In future I would probably tumble for four hours with (media 1) and maybe add a polish or jewelers rouge. Probably jewelers rouge.
I would then tumble for two hours in (media2) with jewelers rouge added.
The results are acceptable to me but I know some other people feel the need to be able to use there brass as shaving mirrors so obviously this will not suit them.
Re: Tumbling brass
(media 2) Results
https://www.ebay.co.uk/itm/401116353315
(media 2) is 25/52 grit. Does not block primer pocket flash hole.
The pictures don't do them justice they are not bad in the flesh.
(media 1) does the job but blocks primer pocket flash holes. (media 2) is 25/52 grit. Does not block primer pocket flash hole.
The pictures don't do them justice they are not bad in the flesh.
Re: Tumbling brass
Has anyone tried mixing walnut media and pins?
I'm not sure if there would be an advantage, just curious
I'm not sure if there would be an advantage, just curious

Re: Tumbling brass
One is a dry process and the other a wet process. Pins won't work dry, and walnut won't work wet. I can't see an advantage.Gazza wrote:Has anyone tried mixing walnut media and pins?
I'm not sure if there would be an advantage, just curious
..
Re: Tumbling brass
Why would you use media 1 when it blocks the flash holes (and creates more work to clear them)?Alpha1 wrote:In future I would probably tumble for four hours with (media 1) and maybe add a polish or jewelers rouge. Probably jewelers rouge. I would then tumble for two hours in (media2) with jewelers rouge added.
Why would you use 2 different media, so you have to separate twice (again more unnecessary work)?
Why choose jeweller's rouge - the messy dusty option?
And if you don't really care about the finish, why tumble for 6 hours (plus the 2 media separations & blocked flash hole clearing)?
..
Re: Tumbling brass
Because I can.
Jewelers rouge is not messy its a powder you just add to the media. The next time I clean cases is probably months away as I said its not high on my list of priorities. It hardly takes up lots of my time.